How thick an e.max crown needs to be, and why it matters

What research shows about how thick an e.max crown needs to be, why thin ceramic depends on bonding, and how these crowns have lasted in long-term clinical records.

Dr James Tran, dentist at Lumi Dental Melrose Park

Dr James Tran

November 12, 2026 · Patient Education · 9 min read

Advice on how thick the biting surface of a lithium disilicate crown, the material family that includes e.max, should be on a molar has moved over the years. A 2022 laboratory study described the earlier recommendation as 1.5 mm and the newer one as 1.0 mm, and tested crowns as thin as 0.8 mm (Jurado and colleagues, Dental Materials Journal, 2022). Small differences in thickness matter, because the space for the ceramic usually comes from shaping the tooth. This article looks at what the research says about thin e.max crowns, why the way the crown is fixed to the tooth changes the answer, and how these crowns have performed in long-term clinical records.

The thickness of the ceramic is a large part of its strength

e.max is a lithium disilicate glass ceramic. At Lumi we use e.max and also offer zirconia. Our article on glass ceramic and zirconia crowns compares them side by side, and our piece on zirconia grades explains how they differ.

Researchers group ceramic crowns by thickness. A 2026 review defined thin crowns as 0.6 to 0.9 mm and ultrathin crowns as 0.5 mm or less (Alghauli and Alqutaibi, Journal of Prosthodontics, 2026). Recommended thicknesses for back teeth, such as the 1.0 to 1.5 mm described above, are greater than this, which is why the tooth usually needs to be reduced before the crown is made.

Thinner crowns break at lower loads in the laboratory

Several laboratory studies have loaded lithium disilicate molar crowns of different thicknesses until they broke. Results vary with the test method, but they point the same way: less ceramic usually means a lower breaking load, although many thinner crowns still withstood more force than normal chewing.

StudyWhat was testedMain finding
Nawafleh and colleagues, Journal of Advanced Prosthodontics, 2017Molar crowns on a standard preparation (2 mm biting surface, 1.5 mm walls) compared with a reduced preparation (1 mm biting surface and walls, 0.8 mm margin)Reducing the preparation significantly lowered the fracture load, before and after simulated ageing
Jurado and colleagues, Dental Materials Journal, 2022Milled molar crowns at 1.5, 1.0 and 0.8 mm after fatigue loadingFracture resistance fell as thickness fell, but all three exceeded the reported maximum bite force for the first molar region
Spitznagel and colleagues, Journal of Esthetic and Restorative Dentistry, 2024Bonded e.max crowns and partial coverage restorations at 1.5, 1.0 and 0.5 mm on composite dies, with long fatigue loadingEight of the twelve 0.5 mm crowns showed cracks after fatigue; partial coverage designs had higher failure loads than crowns at 0.5 and 1.0 mm
Tartuk and colleagues, Materials, 2026Milled e.max and 3D-printed resin crowns at 0.5, 1.0 and 1.5 mm on extracted molarsThickness and material both affected strength; the authors suggested at least 1.0 mm as a reliable threshold for back teeth
ElSharkawi and colleagues, Journal of Contemporary Dental Practice, 2026Margin thickness of 0.5 mm compared with 1 mm on extracted molars, for two lithium disilicate ceramics and a hybrid ceramicMargin thickness made no significant difference to fracture resistance

These are laboratory tests on small numbers of crowns, often five to twelve per group. They are useful for comparing designs, but a machine pressing on a crown does not reproduce years of chewing, temperature changes and grinding.

How the crown is fixed changes the picture

The 2026 review by Alghauli and Alqutaibi included 14 laboratory studies of thin and ultrathin ceramic crowns. Thin and ultrathin crowns had significantly lower fracture resistance than thick crowns. Crowns fixed with conventional cement were significantly weaker than those bonded with resin cement, and with adhesive resin bonding, fracture resistance was similar regardless of crown thickness or material. The authors also noted that the fatigue results were conflicting, which they suggested may reflect differences in methods or cementation.

In practical terms, these laboratory findings suggest a thin glass ceramic crown depends on being bonded to the tooth. That is one reason bonding steps receive so much attention. Our article on immediate dentine sealing explains one of these steps, which Lumi uses for indirect bonded restorations, and our piece on how zirconia crowns are bonded covers the different approach that zirconia needs.

Long-term clinical records for e.max crowns

The clinical evidence is more reassuring than the laboratory numbers might suggest, with some limits on where it comes from.

  • A systematic review of 12 clinical studies reported a 5-year cumulative survival of 97.8% for lithium disilicate single crowns, and 96.7% over 10 years, the 10-year figure coming mainly from one study. Most failures were in back teeth (Pieger and colleagues, Journal of Prosthetic Dentistry, 2014).
  • In a private practice study of 1,960 pressed e.max complete coverage restorations, the estimated 10-year cumulative survival was 99.6%. Seven failed, and five of those seven were molars (Malament and colleagues, Journal of Prosthetic Dentistry, 2019).
  • In 2,392 posterior pressed e.max restorations from the same practice, estimated survival at 16.9 years was 96.49%. The authors found that the thickness of the restoration had no significant effect on survival (Malament and colleagues, Journal of Prosthetic Dentistry, 2021).
  • In 53 people with severe tooth wear who received 662 pressed e.max restorations, six failed over a follow-up of up to 14 years, an overall survival of 98.6% (Margvelashvili-Malament and colleagues, Journal of Prosthetic Dentistry, 2025).

The three Malament papers come from one research group working in private practice with pressed, bonded e.max. Results in other settings, with other workflows, may differ.

Not every lithium disilicate ceramic behaves the same way

A 2026 study from Göttingen examined 100 crowns at least two years after they were placed: 50 made from a different CAD/CAM lithium disilicate based glass ceramic, and 50 from a translucent multilayer zirconia. Two-year survival was 82.0% for the glass ceramic crowns, with 10 bulk fractures, and 100% for the zirconia crowns (Hausdörfer and colleagues, Dental Materials, 2026). This was not an e.max study, which is the point: results for one brand and processing method cannot simply be assumed for another, even when the material family has the same name.

Grinding and e.max molar crowns

People who grind their teeth often ask whether e.max is strong enough. A trial of 109 people needing a molar crown randomly allocated the crown material, monolithic lithium disilicate or zirconia, and measured sleep bruxism with a questionnaire, an examination and a portable muscle recording device. Night guards were not allowed during the study. After three years there were no technical complications in any group, and survival was 96.3% for lithium disilicate crowns in people with sleep bruxism and 100% in those without, a difference that was not statistically significant (Bömicke and colleagues, Journal of Dentistry, 2026). Three years is a short time for a crown, and the groups were small, so this is encouraging rather than conclusive. Our guide to grinding and night guards covers protecting teeth and restorations.

When there is not much room for the ceramic

Sometimes a tooth is short, worn or already heavily filled, and there is little room to give a crown its usual thickness without removing more tooth. The options then depend on the tooth. In the Spitznagel laboratory study, partial coverage designs had higher failure loads after fatigue testing than full crowns at the same thin thicknesses. Lumi provides onlays, and our articles on table-top onlays for worn back teeth and onlays or crowns after a root canal look at the evidence for these.

Treatment room at Lumi Dental with a 3D scan of the teeth displayed on the screen
A 3D scan of the teeth on screen in one of Lumi's treatment rooms.

For dentists: thin lithium disilicate and the luting choice

If a lithium disilicate crown preparation ends up with less occlusal clearance than planned, the luting protocol becomes part of the strength calculation. In the 2026 meta-analysis by Alghauli and Alqutaibi, conventionally cemented thin crowns were significantly weaker than resin bonded ones, while adhesively bonded crowns showed similar fracture resistance across thicknesses and materials. For molars with very limited space, the Spitznagel group found, on composite dies, that non-retentive partial coverage designs outperformed full crowns of the same ceramic thickness at 0.5 and 1.0 mm, and that eight of twelve 0.5 mm crowns showed cracks after fatigue.

The limits are real. All of this is laboratory data, fatigue protocols differ between studies, and the review itself describes conflicting fatigue results. The long-term clinical series that found no effect of thickness on survival comes from one research group using pressed, bonded e.max. Treat thin bonded lithium disilicate as a reasonable option on a well chosen tooth, not as a reason to under-prepare routinely.

Questions about e.max thickness

Can an e.max crown be made thinner to save more of my tooth?

Sometimes. Laboratory studies show that thinner crowns break at lower loads, but crowns of about 1 mm, and in one study 0.8 mm, still resisted more than normal biting forces when tested. How thin is reasonable depends on the tooth, the bite and how the crown is bonded. In some cases a partial coverage restoration may keep more tooth than a thin full crown.

Is e.max or zirconia better if I grind my teeth?

In the three-year randomised trial by Bömicke and colleagues, sleep bruxism made no detectable difference to the survival of either monolithic lithium disilicate or zirconia molar crowns, and survival was high in both. Longer follow-up is still needed, and the choice also depends on the space available and how the tooth looks.

Why do results differ between studies of lithium disilicate?

Studies use different products, processing methods (pressed or milled), thicknesses, test machines and bonding protocols. The Göttingen study of a CAD/CAM lithium disilicate based ceramic found much lower two-year survival than the long-term pressed e.max series, which shows why the specific material matters.

Sources

  • Jurado CA and colleagues. CAD/CAM lithium disilicate ceramic crowns: effect of occlusal thickness on fracture resistance and fractographic analysis. Dental Materials Journal, 2022. PubMed 35793941
  • Alghauli MA and Alqutaibi AY. Mechanical behavior and laboratory survival of thin and ultrathin ceramic crowns: a systematic review and meta-analysis. Journal of Prosthodontics, 2026. PubMed 41084098
  • Nawafleh NA and colleagues. Fracture load and survival of anatomically representative monolithic lithium disilicate crowns with reduced tooth preparation and ceramic thickness. Journal of Advanced Prosthodontics, 2017. PubMed 29279760
  • Spitznagel FA and colleagues. Minimally invasive CAD/CAM lithium disilicate partial-coverage restorations show superior in-vitro fatigue performance than single crowns. Journal of Esthetic and Restorative Dentistry, 2024. PubMed 38009505
  • Tartuk BK, Altıntaş E and Şengül M. Fracture resistance of CAD/CAM lithium disilicate and 3D-printed resin crowns with varying occlusal thickness: an in vitro study. Materials, 2026. PubMed 41900671
  • ElSharkawi NM, Sherif RM and Rabie KA. Fracture resistance of lithium disilicate and hybrid ceramic crowns with two finish line thicknesses: an in vitro study. Journal of Contemporary Dental Practice, 2026. PubMed 42878325
  • Pieger S, Salman A and Bidra AS. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review. Journal of Prosthetic Dentistry, 2014. PubMed 24674802
  • Malament KA and colleagues. Ten-year survival of pressed, acid-etched e.max lithium disilicate monolithic and bilayered complete-coverage restorations. Journal of Prosthetic Dentistry, 2019. PubMed 30955942
  • Malament KA and colleagues. Comparison of 16.9-year survival of pressed acid etched e.max lithium disilicate glass-ceramic complete and partial coverage restorations in posterior teeth. Journal of Prosthetic Dentistry, 2021. PubMed 33010922
  • Margvelashvili-Malament M and colleagues. Over 14-year survival of pressed e.max lithium disilicate glass-ceramic complete and partial coverage restorations in patients with severe wear. Journal of Prosthetic Dentistry, 2025. PubMed 39084921
  • Hausdörfer T and colleagues. Clinical performance of CAD/CAM-fabricated lithium-disilicate-based glass ceramic vs. multilayer zirconia crowns after a minimum observation period of two years. Dental Materials, 2026. PubMed 42624766
  • Bömicke W and colleagues. Ceramic crowns and sleep bruxism: 3-year results of a randomized controlled trial. Journal of Dentistry, 2026. PubMed 41967567

If you have been told a tooth needs a crown and want to talk through materials and how much tooth would be involved, you can book an appointment at our Melrose Park practice or read more about crowns and bridges at Lumi.

This article is general information only and is not a substitute for an in-person assessment by a dental professional.

Dr James Tran, dentist at Lumi Dental, Melrose Park

Written by Dr James Tran

Dr James Tran (BDent, University of Sydney; Graduate Diploma in Oral Implants) is a general dentist at Lumi Dental in Melrose Park. The team writes these articles to give clear, evidence-based dental information to help you make informed decisions about your care.

Inside Lumi Dental, Melrose Park

New patients

Your first visit is $149

A full 60 minute first visit with a check-up, clean, X-rays and a treatment plan. Usually $654, offer ends 31 December 2026. With most health funds there is no gap.

Open Monday to Saturday, and until 9:30pm on Thursdays. Free undercover parking at Melrose Central.