A lithium disilicate crown, often known by the brand name e.max, can reach the mouth by two quite different routes. In one, a technician shapes the crown in wax and heat-softened ceramic is pressed into a mould made from that wax pattern. In the other, the crown is designed on a computer and cut from a ready-made block. Systematic reviews comparing the two have judged the fit at the crown edge clinically acceptable either way, and have not found a consistent difference between them.
Two ways to make the same material
Pressing. The crown is modelled in wax on a model of the tooth. The wax is set in a heat-resistant investment, burnt out, and a softened ingot of lithium disilicate is pressed into the space it leaves. This is known as the lost-wax technique.
Milling. The tooth is scanned, or a model is scanned, and the crown is designed with software. A milling machine cuts it from a block of the ceramic. Milling can be done in a dental laboratory, at a central production site, or chairside in the surgery.
The material in both cases belongs to the same family, but the processing differs, and so can the details of the final crown. Our article on how a crown is made in the dental laboratory covers the wider process.
Fit at the edge of the crown is similar
The marginal gap is the small space between the edge of the crown and the tooth. It is a common measure of how well a crown fits.
Three reviews have pooled the studies on this question:
- A 2023 meta-analysis of nine studies, seven in the laboratory and two in patients, found no significant difference within either group of studies. Combining both groups did show a difference, but the authors judged both methods clinically acceptable (Sanches and colleagues, Journal of Prosthetic Dentistry).
- A 2024 meta-analysis of single crowns made with IPS e.max Press or IPS e.max CAD found pressed crowns had a better average marginal fit, but the difference was not statistically significant. Of 18 included studies, 17 were laboratory studies (Pachiou and colleagues, International Journal of Computerized Dentistry).
- A 2026 meta-analysis of internal fit, the space under the crown, found no significant difference overall, with very high variation between studies. When five methodologically different studies were set aside, pressed crowns fitted about 19 micrometres more closely on the inside (Pachiou and colleagues, Journal of Prosthodontic Research). The authors concluded the evidence does not show a consistent difference.
These reviews did not show whether a difference of this size changes how long a crown lasts.
What a trial in patients found
A University of Zurich and Geneva team made five lithium disilicate crowns for the same tooth in each of 10 people: four through digital workflows and one by the conventional route of a silicone impression, wax-up and pressing (Zeltner and colleagues, Journal of Prosthetic Dentistry, 2017). The differences in marginal gap between workflows were not statistically significant. The pressed crowns had significantly smaller gaps at the cusp tips and over the biting surface than crowns from all four digital workflows. The authors also concluded that chairside milling gave a less favourable fit than milling at a central production site.
Because each workflow also had its own impression method, a scan or a silicone impression, the trial tested whole workflows rather than milling against pressing alone. The same team reported that the technician's total active working time was about 148 minutes for the pressed crown, compared with 74 to 92 minutes for the digital workflows (Sailer and colleagues, Journal of Prosthetic Dentistry, 2017).

Strength in laboratory tests
In a laboratory study of lower premolar crowns 1.5 mm thick, 15 crowns per group from several pressed and milled lithium disilicate products were bonded to metal dies and loaded to fracture (Lim and colleagues, Odontology, 2020). The milled crowns had a higher Weibull modulus, a measure of how consistent strength is from one crown to the next, than the pressed crowns (about 9 to 14, compared with about 5). In other words, the strength of the milled crowns varied less from crown to crown.
In thin veneer-style specimens 0.6 mm thick, cemented to composite bars and bent until they broke, pressed and milled lithium disilicate had similar flexural strength (Rizzante and colleagues, Quintessence International, 2020). In the same study, a thinner 0.4 mm core with a 0.2 mm layer of glass-ceramic on top had lower strength for both methods.
These were tests on small numbers of samples in a machine. They show what each method can do under controlled conditions, not how crowns behave over years of chewing.
For veneers, the evidence leans slightly towards pressing
A 2025 systematic review of lithium disilicate veneers on front teeth included eight studies (Sudharson and colleagues, Journal of Esthetic and Restorative Dentistry). Only five of these compared the two methods directly. The review reported better marginal adaptation and higher long-term survival with pressed veneers, and better internal fit and a more efficient workflow with milled veneers. Colour match was acceptable with both. Only one included trial was at low risk of bias, and most outcomes were rated low or very low certainty.
A randomised clinical trial that compared milled and pressed lithium disilicate veneers in patients concluded that both showed high accuracy and similar results (Soares-Rusu and colleagues, Operative Dentistry, 2021).
Our post on e.max, zirconia and feldspathic veneers compares the materials themselves.
The largest long-term series used pressed crowns
One of the largest long-term series on lithium disilicate comes from one research group in private practice using pressed, acid-etched e.max. In 1,960 complete-coverage restorations, monolithic and layered, in 556 patients, estimated cumulative survival at 10 years was 99.6% (Malament and colleagues, Journal of Prosthetic Dentistry, 2019). That tells us pressed lithium disilicate can perform well over a decade in that setting. It does not show that milled crowns would do worse, because they were not compared.
Our article on e.max crown thickness looks at this series and others in more detail.
What this means for a patient
| Question | Pressed | Milled |
|---|---|---|
| Marginal fit | Clinically acceptable; better on average in one review, but not significantly | Clinically acceptable; no consistent significant difference from pressed |
| Internal fit | Closer over the cusps and biting surface in one clinical trial | No consistent difference overall in a 2026 review |
| Consistency of strength | Lower Weibull modulus in one lab study | Higher Weibull modulus in the same study |
| Technician time | Longer in a clinical workflow study | Shorter in the same study |
| Long-term data | Large 10-year series from one group | No comparable series among the studies reviewed here |
Taken together, the studies do not show that one method is clearly better for crowns. Both can produce a crown that fits within accepted limits. Asking how your crown will be made is a reasonable question, and so is asking why that route suits your tooth.
Crowns and veneers at Lumi
Lumi uses e.max (lithium disilicate) and also offers zirconia, and the practice has an in-house lab with 3D printing alongside a 3D intraoral scanner. After an examination you will usually receive a written treatment plan, often by email. See our crowns and bridges page or porcelain veneers page for more, and current deals for consult offers.
For dentists: judging a lithium disilicate restoration at try-in
Check the inside, not just the margin. In the Zeltner trial the marginal gap did not differ significantly between workflows, but the pressed crowns had significantly smaller internal gaps at the cusp tips and over the occlusal surface than all four digital workflows, and the authors concluded that chairside milling fitted less favourably than central milling. A laboratory onlay study found the same pattern, with larger internal gaps under CAD/CAM onlays than under pressed onlays (Guess and colleagues, Journal of Dentistry, 2014). On this evidence, a margin that looks closed does not confirm that the internal fit is equally close. The limits: both studies were small, fit was measured on replicas or sectioned specimens rather than at try-in, and neither showed an effect on how long restorations last.
Allow for the marginal gap to increase once the restoration is bonded. In the same study of 72 extracted lower molars restored with IPS e.max Press, a second pressed ceramic or IPS e.max CAD onlays, adhesive luting with a dual-cure resin cement significantly increased the marginal gap in every group, while the chewing simulation and temperature cycling that followed did not. Mean marginal gaps stayed within the 100 micrometre limit the authors used as clinically acceptable. The limits of this tip: it rests on one laboratory study of onlays rather than crowns, with one cement, and how the extra gap affects outcomes in patients is not known.
Common questions
Is a same-day crown the same as a lab-milled crown?
Both are milled, but the setting differs. In the Zurich trial, the authors concluded that chairside milling gave a less favourable fit than central milling, although the differences in marginal gap between workflows were not statistically significant. Our digital scan vs impression article explains the scanning step.
Will I be able to tell the difference by looking?
In the veneer review, colour match was within clinically acceptable limits with both methods, although the certainty of that evidence was low. The studies reviewed here did not test whether people could see a difference.
Does one method last longer?
The studies reviewed here include no head-to-head trial of crown survival. The veneer review reported higher long-term survival with pressed veneers, at low certainty. The largest long-term crown series reviewed here used pressed e.max, so it cannot show how milled crowns compare.
Sources
- Sanches IB and colleagues. Marginal adaptation of CAD-CAM and heat-pressed lithium disilicate crowns: a systematic review and meta-analysis. J Prosthet Dent. 2023. PubMed 34147239
- Pachiou A and colleagues. Evaluation of the marginal fit of lithium disilicate single crowns fabricated with the conventional (IPS e.max Press) and CAD/CAM (IPS e.max CAD) methods: a systematic review and meta-analysis. Int J Comput Dent. 2024. PubMed 37477084
- Pachiou A and colleagues. Internal fit of lithium disilicate crowns: a systematic review and meta-analysis comparing heat-pressed and CAD-CAM-milled fabrication methods. J Prosthodont Res. 2026 (online ahead of print). PubMed 41850865
- Zeltner M and colleagues. Randomized controlled within-subject evaluation of digital and conventional workflows for the fabrication of lithium disilicate single crowns. Part III: marginal and internal fit. J Prosthet Dent. 2017. PubMed 27677220
- Sailer I and colleagues. Randomized controlled within-subject evaluation of digital and conventional workflows for the fabrication of lithium disilicate single crowns. Part II: CAD-CAM versus conventional laboratory procedures. J Prosthet Dent. 2017. PubMed 28024819
- Lim CH and colleagues. Evaluation of fracture strength for single crowns made of the different types of lithium disilicate glass-ceramics. Odontology. 2020. PubMed 31564006
- Rizzante FAP and colleagues. Flexural strength of minimum thickness ceramic veneers manufactured with different techniques. Quintessence Int. 2020. PubMed 32128525
- Sudharson NA and colleagues. Clinical performance and survival outcomes of milled versus pressed lithium disilicate veneers: a systematic review. J Esthet Restor Dent. 2025. PubMed 41024714
- Soares-Rusu I and colleagues. Clinical evaluation of lithium disilicate veneers manufactured by CAD/CAM compared with heat-pressed methods: randomized controlled clinical trial. Oper Dent. 2021. PubMed 33882132
- Malament KA and colleagues. Ten-year survival of pressed, acid-etched e.max lithium disilicate monolithic and bilayered complete-coverage restorations. J Prosthet Dent. 2019. PubMed 30955942
- Guess PC and colleagues. Marginal and internal fit of heat pressed versus CAD/CAM fabricated all-ceramic onlays after exposure to thermo-mechanical fatigue. J Dent. 2014. PubMed 24161516